Every welded joint in a steel building should be made to a proven procedure. The documents that prove it - the welding procedure specification (WPS) and the procedure qualification record (PQR) - are the buyer's evidence that the welding is controlled, not improvised.
1. What a WPS is
A WPS is the recipe: the welding process, consumable, current, voltage, travel speed, number of passes, preheat and interpass temperature, and the joint preparation. It tells the welder exactly how to make the joint.
2. What a PQR is
A PQR is the test record that proves the WPS works. A test joint is welded to the proposed procedure, then cut and tested - tensile, bend, impact, hardness, depending on the application. If the results pass, the procedure is qualified.
3. Why buyers should care
Without qualification, welding quality depends on whoever holds the torch that day. With it, the procedure is fixed, tested and repeatable - and the records show it was followed. This matters most for thick plates, high-strength steels, low temperatures and fatigue-loaded joints.
4. What the documents cover
A qualified procedure covers a range of thicknesses, positions, materials and consumables. Outside that range, a new qualification is needed. Ask whether your thickest plate and your most critical joint fall inside the qualified range.
5. The paper trail
WPS for each joint type.
PQR supporting each WPS.
Consumable certificates.
Welder qualification records.
Inspection reports for production welds.
6. What to ask your supplier
Can I see the WPS and PQR for my joint types?
Do my thicknesses and steel grades fall within the qualified range?
Are consumables certified and stored correctly?
Are production welds inspected to the specified level?
In short: WPS and PQR turn welding from craft into a controlled, repeatable process. Ask for them, check that your steel and thickness are covered, and keep them in the project file.