How to Improve the Corrosion Resistance of Steel - structured Buildings in Coastal Areas?

Jun 16, 2026

Leave a message

In coastal areas, the high air humidity and strong salt - fog corrosion pose extremely high requirements for the corrosion resistance of steel - structured buildings. To ensure the long - term stable use of steel - structured buildings in the coastal environment, comprehensive and effective anti - corrosion measures need to be taken.

1. Rational Selection of Steel

Weathering SteelGive priority to weathering steel, such as Q355NH. This type of steel can form a dense and stable rust layer in the atmospheric environment, which hinders the further erosion of oxygen and moisture to the steel substrate, and has good atmospheric corrosion resistance. Compared with ordinary steel, the corrosion resistance of weathering steel in coastal areas can be increased by 2 - 3 times, effectively extending the service life of the steel structure.

Hot - dip Galvanized SteelHot - dip galvanized steel has a uniform and strongly adherent zinc layer on its surface. The zinc layer can provide cathodic protection to the steel. Even if the zinc layer is partially damaged, the surrounding zinc can still protect the exposed steel through electrochemical action. In coastal areas, the thickness of the hot - dip galvanized layer generally needs to reach 80 - 100μm, which can significantly increase the corrosion - resistant life of the steel.

2. Surface Pretreatment

Mechanical Rust RemovalBefore painting or other anti - corrosion treatments, mechanical rust - removal methods such as sandblasting and shot - peening are used to thoroughly remove impurities such as rust, scale, and oil from the steel surface. Sandblasting can create a uniform roughness on the steel surface, increasing the adhesion between the coating and the steel. The cleanliness of the steel surface after sandblasting should reach level Sa2.5 or above, that is, there should be no visible grease, dirt, scale, rust, and paint coatings on the steel surface, and any remaining traces should only be slight color spots in the form of dots or stripes.

Chemical TreatmentChemical methods such as pickling and phosphating can be used for the surface pretreatment of steel. Pickling can remove rust and scale from the steel surface, and phosphating treatment forms a phosphate protective film on the steel surface, further improving the adhesion and corrosion resistance of the coating. The steel after chemical treatment should be promptly subjected to subsequent anti - corrosion treatments to prevent re - rusting.

3. Anti - corrosion Coating System

PrimerSelect high - performance primers, such as zinc - rich primers. Zinc - rich primers contain a large amount of zinc powder, which can provide cathodic protection to the steel and at the same time provide a good adhesion foundation for the intermediate coat and topcoat. In coastal areas, the dry film thickness of zinc - rich primers generally needs to reach 80 - 100μm.

Intermediate CoatThe intermediate coat mainly serves to increase the coating thickness, improve the shielding performance and adhesion of the coating. Commonly used intermediate coats include epoxy micaceous iron oxide intermediate coats, which have good abrasion resistance, water resistance, and rust - proof performance. The dry film thickness of the intermediate coat is generally controlled at 100 - 150μm.

TopcoatThe topcoat should have excellent weather resistance, salt - fog resistance, and water resistance. Acrylic polyurethane topcoats, fluorocarbon topcoats, etc. can be selected. Fluorocarbon topcoats have extremely high weather resistance, can maintain color and luster for a long time in the harsh coastal environment, and have good anti - chalking performance. The dry film thickness of the topcoat is generally 60 - 80μm. The total dry film thickness of the entire anti - corrosion coating system should reach 250 - 350μm.

4. Treatment of Nodes and Gaps

Node SealingNode parts of the steel structure, such as bolt - connected nodes and welded nodes, are prone to accumulate moisture and salt, causing corrosion. These nodes should be sealed with sealants to prevent the intrusion of corrosive media. For example, at bolt - connected nodes, silicone sealants can be used to fill the gaps between bolts and connecting plates to ensure the sealing of the nodes.

Gap FillingFor the gaps between steel - structure components, such as the connections between steel beams and columns, and between purlins and steel beams, appropriate materials should be used for filling. Fire - proof, moisture - proof, and anti - corrosion sealant strips or sealants can be used to fill the gaps and form a continuous sealing layer, preventing moisture and salt - fog from entering the gaps and causing corrosion.

5. Regular Maintenance and Inspection

Regular InspectionEstablish a regular inspection system, and conduct a comprehensive inspection of the steel - structured building every 1 - 2 years. Focus on checking the integrity of the coating, whether there is damage, peeling, chalking, etc., and the sealing condition of the node parts. For damaged coating parts found, they should be repaired in a timely manner.

Non - destructive TestingEvery 3 - 5 years, use non - destructive testing techniques such as ultrasonic testing and magnetic particle testing to detect key parts of the steel structure to check for internal corrosion, cracks, and other defects. Once problems are found, timely repair measures should be taken to ensure the safety performance of the steel structure.

Coating MaintenanceAccording to the aging degree of the coating and the inspection results, regularly maintain the coating of the steel structure. Generally, repaint the coating every 5 - 8 years to maintain the effectiveness of the anti - corrosion coating and extend the service life of the steel - structured building.